Round pits, a dull patch, and a thin spot can all show up on the same line. Start with what you can see, then check the process step most likely to explain it. For a powder coat color mismatch, compare film thickness and cure on both parts before changing the powder.

Defects and fixes · Photo comparison · RAL color matching · Send an inquiry

Powder coat defects and how to fix them

Use the close-ups to identify the symptom. Start with the listed checks and confirm the cause on a test part before changing production settings.

Defect and appearance What to check and how to fix it
Small pits scattered across a blue-gray coatingCraters / fisheyesRound depressions in the finish. Start with contamination. Check the part for oil, fingerprints, or release agent. Restore the cleaning step and check the gun air supply for oil or moisture. Spray a clean test panel to see whether the craters recur.
White coating with a continuous rippled textureOrange peelAn unintended wavy texture on a smooth finish. Measure dry film thickness. Bring it into the powder's technical data sheet (TDS) range. If film build is uneven, steady the gun distance, pass speed, and overlap. If thickness is in range, verify the part's heat-up and cure profile.
Yellow coating with a cluster of small point defectsPinholes / bubblesTiny openings or raised blisters. Check moisture and outgassing. Dry parts after pretreatment and verify that the air dryer works. If defects recur on porous castings, test a supplier-approved pre-bake or an outgassing-tolerant powder on a sample part.
Gray coated metal pieces with flakes missing from the surfacePoor adhesionFilm lifts, chips, or peels from the part. Verify pretreatment and cure. Check cleaning, degreasing, and substrate pretreatment. Record the actual part metal temperature and time against the TDS. Retest adhesion on a fresh panel using the method specified for the job.
Two adjacent gray coated panels with different apparent shadesColor variationParts or areas appear lighter or darker. Compare like-for-like samples. Inspect under the same lighting. Check the powder lot, film thickness, and cure. Keep gun distance and spray pattern consistent. If feed varies, check the hopper's fluidizing air and the gun's powder and air settings.
Light gray coated surface with scattered raised specksDirt or inclusionsScattered specks or bumps in the film. Run a clean-powder test. Use fresh powder on a clean panel. If specks persist, inspect the booth, hooks, hopper, and feed path for debris or powder left from a previous run. Clean the area and repeat the test.
Red coating with uneven reflections around a bright highlightGloss lossA dull or uneven sheen on the cured finish. Profile the oven with a representative part. Check actual part metal temperature and time against the TDS. Compare film thickness and gloss with the approved panel before adjusting the oven or changing the powder.
Orange powder coat with a gray area showing through thin coveragePoor coverage / low depositionThe substrate shows through thin or patchy areas. Check grounding, then the gun. Inspect the hooks and their contact points. If powder deposits unevenly, check the spray pattern, feed, and gun settings. If the film builds evenly but the substrate still shows, compare thickness and hiding power against the TDS and approved panel.

Process checks draw on the IFS Coatings and PPG troubleshooting guides. Use the data sheet for your specific powder and equipment.

Powder coat defects in close-up

Small pits scattered across a blue-gray coating

Craters / fisheyes

White coating with a continuous rippled texture

Orange peel

Yellow coating with a cluster of small point defects

Pinholes / bubbles

Gray coated metal pieces with flakes missing from the surface

Poor adhesion

Two adjacent gray coated panels with different apparent shades

Color variation

Light gray coated surface with scattered raised specks

Dirt or inclusions

Red coating with uneven reflections around a bright highlight

Gloss loss

Orange powder coat with a gray area showing through thin coverage

Poor coverage

Use these close-ups to compare surface symptoms. The orange sample was retouched to remove handwritten markings.

How to match a RAL powder coat color

Specify the RAL color code, gloss level, and surface texture on the same order. Use a physical RAL reference to communicate the target shade, then approve a coated sample on the intended substrate under agreed lighting. Keep the sample as the production reference.

If a production part looks lighter or darker than the approved panel, compare the two under the same light. Check that the powder lot and finish match the order. Measure film thickness at comparable points, including corners or recesses when coverage looks thin. Check the cure record before asking for a color adjustment. For material planning, see powder coating coverage per kg.

How to confirm a fix before restarting the run

  1. Keep a reference part. Mark where the defect appeared. Record the powder lot, substrate, pretreatment, spray settings, film thickness, and cure profile.
  2. Change one variable. Use the table to choose the first check. Run a test part with the same substrate and geometry so you can compare results at the same spot.
  3. Check the cured part against the job spec. Confirm the required appearance, color, gloss, and film thickness. If adhesion was the issue, repeat the specified adhesion test before releasing the run.

Find more from Chengwei Powder Coatings on our YouTube channel.

Request a RAL powder coat sample or quote

Send your RAL code, desired gloss and texture, substrate, indoor or outdoor use, and estimated order quantity. If you are troubleshooting a defect, include a close-up photo, the measured film thickness, and the cure profile if available.

Send a powder coating inquiry

Send Inquiry